Among the many acids, only concentrated nitric or sulfuric acid or aqua regia (a mixture of nitric and hydrochloric acids) assault germanium appreciably. While aqueous caustic remedies generate tiny impact on it, germanium dissolves rapidly in molten sodium hydroxide or potassium hydroxide, thus forming the respective germanates.It really is brittl